When sourcing mold steel, the biggest risk is not the price. It is receiving the wrong grade, mixed heat numbers, or steel below hardness spec—problems often found only in finish machining or at first trial, when the labor and lead time of an entire mold are already lost. The “ID card” of your mold steel is the MTC (Mill Test Certificate, also called MTR).
What Is a Mill Test Certificate?
An MTC is a quality document issued by the mill with the material, recording the grade, heat number, chemical composition, mechanical properties and heat-treatment condition. It traces every block back to a specific heat and serves as the basis for incoming inspection, returns and quality claims.
EN 10204 2.2 vs 3.1 vs 3.2
EN 10204 is the European standard for inspection documents. Four types are common:
· 2.1 — a declaration of compliance: it simply states the order is met, with no test results.
· 2.2 — a test report based on non-specific inspection; batch-level data issued by the mill.
· 3.1 — specific inspection of the products actually delivered; results come from that heat/batch, signed by the mill’s inspection representative independent of the production department, and traceable by heat number. For mold steel, 3.1 is the most common and usually sufficient.
· 3.2 — a 3.1 additionally witnessed and countersigned by the buyer’s representative or an independent third party (SGS, BV, TÜV, Intertek); the highest assurance, reserved for demanding or disputed orders.
In short: 3.1 is the mill’s own test and responsibility; 3.2 adds third-party endorsement.


Figure 1. EN 10204 inspection documents (2.1, 2.2, 3.1, 3.2) and the assurance level each provides.
Fields to Check on an MTC
· Certificate number, issue date and document standard (clearly marked EN 10204 3.1)
· Buyer’s order number and the mill’s heat / cast number
· Product description: grade, specification, form, dimensions, quantity and weight
· Chemical composition (ladle/heat analysis; product analysis if required): C, Mn, Si, Cr, Ni, Mo, etc.
· Mechanical properties: tensile strength, yield strength, elongation; hardness (HB/HRC) and impact values when ordered
· Heat-treatment condition (pre-hardened / annealed / quenched & tempered)
· Inspection department stamp and signature
Whether you order P20/718, S136 or 45# / S45C, verify grade, standard and measured values against the specification limits.
Why It Matters for Mold Steel
Mold steel is expensive and has a long machining cycle. A mixed grade or wrong hardness, often found late in finishing, costs far more than the material itself. The MTC traces every block by heat number—preventing mix-ups and backing returns and claims. Once you decide between pre-hardened and quenched steel, the certificate is the final gate that turns a grade choice into the actual block on the floor.
Incoming Inspection Checklist
1. Confirm the certificate type matches the order (mold steel usually requires EN 10204 3.1).
2. Match the heat number across the MTC, the tag/stamp on the steel and the physical block.
3. Check grade and chemistry against the standard limits.
4. Take hardness readings (Brinell/Rockwell) on site; compare with the heat-treatment condition and certificate.
5. For critical molds: spot-check chemistry with a portable PMI spectrometer; add UT ultrasonic testing or third-party re-test for high requirements.
6. Verify dimensions and appearance (cracks, laps, scale); file the certificate and re-inspection records.


Figure 2. Six-step incoming inspection checklist for mold steel blocks before machining.
Conclusion: Make the MTC a line item in the order and a mandatory step at receiving—not just compare unit price. A missing certificate worth a few dollars can cost an entire mold.
FAQ
Q: What if the supplier only offers 2.2 or no certificate?
A: Specify EN 10204 3.1 in the order. A 2.2 or a copy cannot be traced by heat number; require the original, and set aside suppliers who cannot provide it at the quote stage.
Q: With a 3.1, do I still need to re-inspect?
A: 3.1 is the mill’s self-certification; mix-ups can still occur in transit and stock. At minimum, take hardness readings and check heat numbers for critical molds; add PMI/UT, and specify 3.2 third-party witnessing when needed.
Q: The MTC heat number doesn’t match the stamp—what now?
A: Quarantine and reject it before machining; ask the supplier to verify the source and issue a certificate matching the physical material, or return it. Once machining starts, traceability and claims become far harder.